After Having experimented in Making Perfectly Smooth Surfaces for about a Year now within the Print Process itself, Its time I Capitulate and start putting in some more Work and Sand it all smooth!

Just a bit of an Issue… Whenever I sand Coloured PETG, it looses its Colour and turns into that Broken Plastic White.

As someone who hasn’t had to Fix something like that before, I’m not sure where to even start Fixing this? Can it be Avoided in the Sanding Process, or can the Colour be Regained afterwards?

I have heard of People Treating it with Heat and Vasaline to get the Colour Back, what kind of Methods do you all use and how reliable are they?

  • FuglyDuck@lemmy.world
    link
    fedilink
    English
    arrow-up
    1
    ·
    edit-2
    3 hours ago

    I’ve not used MEK personally, all of my petg parts are structural. What I’m seeing online says 60-80c.

    What I’d do is kick it up by 5c at a time.

    swap in failed test prints and see how that changes things. Keep in mind if you stay in the cold range and give it more time, it might create a better finish.

    Too hot and it’ll start melting.

    Maybe also “priming” the chamber with a heat gun so the air is also warm. (Do this before placing the MEK!)

    Also, a small hole someplace that’ll get covered and a toothpick to lift the part will help retain its shape.