I finally had an area to setup the resin printer i got almost a year ago. Did initial setup, bed leveling, and set out to test with this benchmark I’ve seen around.

It’s an elegoo saturn 2 printer, I’m using CHITUBOX basic as the slicer, all settings were the default it gave for this printer other than adding 0.5 wait time to before lift (default 0) , and bottom layer count to 8 (default 5)

I used the elegoo washing station for 10min then the curing station for 10min. There seem to be a lot of rough lines and the right side line ramp is barely visible at all. Not sure what this suggests needs adjustment and would appreciate some help getting into the correct direction.

I did do some looking around and at least it seems i should try 4 base layers only on this according to one of the places i found it hosted. Other than that I’m not sure how to clean it up more

  • remotelove@lemmy.ca
    link
    fedilink
    English
    arrow-up
    8
    ·
    14 days ago

    Resins have a typical use-time for within a year. Some may last longer, some may not. Some may start to show exposure issues. Some just start to separate or solidify partially. Some resins don’t care at all. (It should be written somewhere on the bottle when the resin was made and when it should be used by.)

    This is a helluva “unknown variable” you are working with, is my point. Resin is the absolute core of any printing functionality (obviously) and print settings are highly dependant on the resins qualities.

    Just because I am so damn picky during my testing and learning process, I would abandon testing with that resin completely and be thankful it even printed a calibration test at all. (I would get a fresh bottle, is what I am saying.)

    However, in the interest of using the resin, I would YOLO the exposure time (increase it) and start printing prototypes or other strange experiments. There is a bunch of things I could test even if using a sub-optimal resin.

    You could spend time with the rest of that bottle and tweak the settings into partial-perfection. How reusable are those settings for future bottles though?

    • LordKitsuna@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      6
      ·
      14 days ago

      That’s a fair point, the date on the bottle says it should be good for another year apparently but it wouldn’t hurt to get a fresh bottle just to be safe. It does look like I would need to fuck with the exposure time regardless since it’s a bright white resin it appears to need longer exposure. I also have a clear resin which apparently needs even more exposure.

      At the very least I know I have good build plate adhesion because God damn some of these have been difficult to get off I actually slightly scratched my build plate in one spot a little bit getting some of them off I need to be more careful and use the plastic spatula not the metal one

      • roofuskit@lemmy.world
        link
        fedilink
        English
        arrow-up
        4
        ·
        edit-2
        13 days ago

        You probably just need to shake the shit out of it. Shake it until you’re too tired, then shake it a lot more.

      • benignintervention@lemmy.world
        link
        fedilink
        English
        arrow-up
        2
        ·
        14 days ago

        Color and age definitely matter too. Each resin should also have a configuration table you can import into the slicer. I use Sirya and they offer data sheets and configs from their website. Not sure which other resin manufacturers do the same

        • LordKitsuna@lemmy.worldOP
          link
          fedilink
          English
          arrow-up
          1
          ·
          13 days ago

          I’ll poke around, it’s an elegoo resin and if I’m not mistaken they at least offer some recommended setting changes somewhere on the website for their resins