I tried 3d print glue stick. washing with alcohol. wash the nozzle, cold pull, higher bed temperature… nothing,
the i has 3 successful prints with the same file, and now for the life of me I can’t get it to work
I tried 3d print glue stick. washing with alcohol. wash the nozzle, cold pull, higher bed temperature… nothing,
the i has 3 successful prints with the same file, and now for the life of me I can’t get it to work
A few things I might consider/think to try:
I don’t have a Bambu, but these are a few of the things I’ve learned with my Monoprice Maker Select v2 and Ankermake M5.
99% of printing issues with PLA are solved with a thin film of glue stick.
IPA does not remove oils, it solubilizes them and then they deposit back down again when it evaporates. Soap and water is better because it removes oils and plasticizers.
You don’t dump alcohol on the plate and then let it evaporate. You put it on a paper towel or microfiber cloth and rub the plate so the oils are transferred to the paper towel.
Dish soap can be problematic because many brands include oils to be soft on hands. Palmolive is named because it has Palm oil in it. Dawn has Palm oil too
(it was solved by washing the plate with soap)
The PLA is a week old, but it was 10$ no brand PLA which might be an issue.
there nozzle might be about a year old,
I’m using 60°, but tried 70°
thanks for your answer